LJAY's Painting and Decorating Services

Common problems

Why Paint Bubbles and Peels, and How to Fix It

Short answer

Paint lifts when it cannot stay bonded to the surface underneath. Moisture is the most common reason, followed by new plaster painted without a mist coat, and paint applied over dust, grease, distemper or shiny old gloss. Find and fix the cause first, then scrape back, repair, prime and repaint.

Bubbling, flaking and peeling: what each tells you

Bubbles or blisters are pockets where the paint has lifted but not yet broken. If they appear soon after painting, trapped moisture or heat is likely. If they come and go, or are filled with water, there is moisture coming from behind or condensing on the surface.

Flaking is when small brittle pieces crack and fall away, typical of old layers that have lost their flexibility or paint sitting on a chalky surface. Peeling, where paint comes away in sheets or strips, usually means it never bonded properly in the first place, for instance on fresh plaster or a glossy surface.

The usual causes

Bathrooms and kitchens produce a lot of steam, and if it cannot escape it condenses on cold walls and ceilings and works its way under the paint. Cold outside walls in bedrooms can suffer the same way. Ordinary emulsion is not designed for this, which is why moisture-resistant finishes and good ventilation matter in these rooms.

New plaster is very absorbent. Painted with full-strength emulsion straight away, the paint skins over the top without soaking in, and later it peels off in sheets. Painting over dust from sanding, kitchen grease or nicotine, old water-based distemper in older houses, or untreated oil gloss on woodwork all give paint nothing firm to hold on to.

Fix the cause before redecorating

Repainting without dealing with the reason only buys a few months. Where condensation is the issue, better ventilation, an extractor fan that works and keeping rooms warm help a great deal. Where water is getting in, such as from a leak, failed seal or rising or penetrating damp, that needs to be traced and fixed by the right specialist.

Louise does not carry out damp treatment, so if the cause looks like damp she will suggest having it checked first. Once the wall is dry and the problem is sorted, the decorating can be done properly.

How the repair is done

All loose and lifting paint is scraped back to a firm edge. The edges are sanded or feathered so they do not show as ridges under new paint, and any damaged plaster is filled. Surfaces are cleaned to remove grease or dust, then the bare and patched areas are primed with a product suited to the surface.

Where scraping has left large bare patches and steps between layers, or the plaster has been damaged, skimming the wall can be quicker and neater than trying to fill everything. Once primed or mist-coated, the wall gets its finishing coats, with a moisture-resistant paint in steamy rooms.

Preventing it next time

Always mist coat fresh plaster with diluted emulsion before normal coats. Clean and lightly sand walls before painting, especially in kitchens. Use a suitable primer over shiny gloss, stained areas or old distemper. Let each coat dry properly before the next, and avoid painting cold, damp walls.

In bathrooms, run the extractor during and after showers and leave the door or window open for a while. Our guide on how long it takes to paint a room explains why drying time between coats is part of a finish that lasts.

Ask for a quote

If paint is lifting in your home, send Louise a photo of the area and a wider view of the room, and mention which room it is and how long ago it was painted. Call 07751 204847 or use the contact page for a quote.

FAQs

Common questions

Why is the paint bubbling in my bathroom?
Almost always because of steam. Moisture condenses on the walls and ceiling and gets under the paint. Better ventilation and a moisture-resistant paint, applied over a properly prepared surface, are the usual cure.
Can I paint straight over peeling paint?
No. New paint will only be as secure as the loose layer beneath it, so it will peel off too. Scrape back to a firm edge, repair and prime first.
Why did paint peel off my new plaster?
Usually because it went on without a diluted mist coat, or before the plaster had dried. The paint sat on the surface instead of soaking in, so it never bonded properly.
Will a stain-blocking primer stop it?
It helps over stains, distemper and some problem surfaces, but it will not stop paint lifting if moisture is still getting into the wall. Sort the cause first, then prime.
Do I need to skim the wall after scraping?
Not always. Small areas can be filled and feathered. If scraping leaves large patches, deep steps or damaged plaster, a skim gives a smoother result.

Have a project in mind?

Let’s give your home a flawless finish.

Request a quote
Call nowGet a quote